swirls in my test e

jediclampet

not a wigger
I just converted 25 g test e using 2% BA and 20% BB. Although this is the same recipe I used for my last batch, today's batch turned out translucent (permitting light to pass through but diffusing it so that objects on the opposite side are not clearly visible: Frosted window glass is translucent but not transparent. ) whereas the previous batch was transparent.

I thought it might be because the gear was not totally dissolved so I heated the vial in boling water for a few minutes but the swirls are still there. Should I filter again or add more solvent or what?
 